Metric UnitsUS Customary Units

Material Properties

Density, g/cm3 1.4 to 1.6
1.3
Elongation at Break, % 2.0 to 5.9
380
Glass Transition Temperature, °C 360
-30
Maximum Temperature: Mechanical, °C 260
110
Specific Heat Capacity, J/kg-K 1130
1350
Strength to Weight: Axial, points 6.5 to 16
3.9
Strength to Weight: Bending, points 16 to 30
12
Tensile Strength: Ultimate (UTS), MPa 37 to 81
18
Thermal Conductivity, W/m-K 0.29 to 1.7
0.25
Thermal Diffusivity, mm2/s 0.18 to 0.95
0.15