Material Properties

Density, g/cm3 1.4 to 1.6
1.2
Elongation at Break, % 2.0 to 5.9
400
Glass Transition Temperature, °C 360
0
Limiting Oxygen Index (LOI), % 40
25
Maximum Temperature: Mechanical, °C 260
120
Strength to Weight: Axial, points 6.5 to 16
2.1
Strength to Weight: Bending, points 16 to 30
8.0
Tensile Strength: Ultimate (UTS), MPa 37 to 81
9.0