Material Properties
Density, g/cm3 | 1.4 to 1.6 | |
1.8 |
Elongation at Break, % | 2.0 to 5.9 | |
300 |
Glass Transition Temperature, °C | 360 | |
-20 |
Limiting Oxygen Index (LOI), % | 40 | |
51 |
Maximum Temperature: Mechanical, °C | 260 | |
220 |
Strength to Weight: Axial, points | 6.5 to 16 | |
1.1 |
Strength to Weight: Bending, points | 16 to 30 | |
4.7 |
Tensile Strength: Ultimate (UTS), MPa | 37 to 81 | |
7.5 |