Density, g/cm3 | 3.7 | |
2.7 |
Dielectric Constant (Relative Permittivity) At 1 Hz | 70 | |
10 |
Electrical Dissipation At 1 MHz | 0.0018 | |
0.00030 |
Flexural Strength, MPa | 75 | |
53 |
Specific Heat Capacity, J/kg-K | 750 | |
950 |
Thermal Conductivity, W/m-K | 3.5 | |
8.0 |
Thermal Diffusivity, mm2/s | 1.3 | |
3.1 |
Thermal Expansion, µm/m-K | 7.0 | |
11 |