MakeItFrom.com
Menu (ESC)

Type 3 Magnetic Alloy vs. ASTM A414 Steel

Type 3 magnetic alloy belongs to the nickel alloys classification, while ASTM A414 steel belongs to the iron alloys. There are 28 material properties with values for both materials. Properties with values for just one material (4, in this case) are not shown.

For each property being compared, the top bar is Type 3 magnetic alloy and the bottom bar is ASTM A414 steel.

Metric UnitsUS Customary Units

Mechanical Properties

Elastic (Young's, Tensile) Modulus, GPa 180
190
Elongation at Break, % 43
15 to 26
Fatigue Strength, MPa 170
140 to 260
Poisson's Ratio 0.31
0.29
Shear Modulus, GPa 70
73
Shear Strength, MPa 380
230 to 370
Tensile Strength: Ultimate (UTS), MPa 550
360 to 590
Tensile Strength: Yield (Proof), MPa 210
190 to 350

Thermal Properties

Latent Heat of Fusion, J/g 290
250
Maximum Temperature: Mechanical, °C 910
400
Melting Completion (Liquidus), °C 1370
1460
Melting Onset (Solidus), °C 1320
1420
Specific Heat Capacity, J/kg-K 450
470
Thermal Expansion, µm/m-K 12
13

Electrical Properties

Electrical Conductivity: Equal Volume, % IACS 2.9
7.2 to 7.3
Electrical Conductivity: Equal Weight (Specific), % IACS 3.0
8.3 to 8.4

Otherwise Unclassified Properties

Base Metal Price, % relative 55
2.2
Density, g/cm3 8.7
7.8 to 7.9
Embodied Carbon, kg CO2/kg material 8.7
1.5 to 1.6
Embodied Energy, MJ/kg 120
20 to 22
Embodied Water, L/kg 220
48

Common Calculations

Resilience: Ultimate (Unit Rupture Work), MJ/m3 190
69 to 130
Resilience: Unit (Modulus of Resilience), kJ/m3 120
100 to 330
Stiffness to Weight: Axial, points 12
13
Stiffness to Weight: Bending, points 22
24
Strength to Weight: Axial, points 18
13 to 21
Strength to Weight: Bending, points 17
14 to 20
Thermal Shock Resistance, points 18
11 to 17