C71500 Copper-nickel vs. N07041 Nickel
C71500 copper-nickel belongs to the copper alloys classification, while N07041 nickel belongs to the nickel alloys. There are 13 material properties with values for both materials. Properties with values for just one material (19, in this case) are not shown.
For each property being compared, the top bar is C71500 copper-nickel and the bottom bar is N07041 nickel.
Metric UnitsUS Customary Units
Mechanical Properties
Elastic (Young's, Tensile) Modulus, GPa | 140 | |
220 |
Tensile Strength: Ultimate (UTS), MPa | 380 to 620 | |
1400 |
Thermal Properties
Melting Onset (Solidus), °C | 1170 | |
1320 |
Specific Heat Capacity, J/kg-K | 400 | |
450 |
Thermal Conductivity, W/m-K | 28 | |
11 |
Thermal Expansion, µm/m-K | 16 | |
12 |
Otherwise Unclassified Properties
Density, g/cm3 | 8.9 | |
8.2 |
Common Calculations
Stiffness to Weight: Axial, points | 8.6 | |
15 |
Stiffness to Weight: Bending, points | 19 | |
25 |
Strength to Weight: Axial, points | 12 to 19 | |
47 |
Strength to Weight: Bending, points | 13 to 18 | |
34 |
Thermal Diffusivity, mm2/s | 7.7 | |
3.0 |
Thermal Shock Resistance, points | 12 to 20 | |
38 |