Metric UnitsUS Customary Units

Material Properties

Electrical Conductivity: Equal Volume, % IACS 7.0
84 to 86
Elongation at Break, % 2.0 to 43
9.0 to 37
Resilience: Ultimate (Unit Rupture Work), MJ/m3 12 to 120
24 to 70
Shear Strength, MPa 250 to 370
150 to 160
Tensile Strength: Ultimate (UTS), MPa 370 to 630
230 to 280
Tensile Strength: Yield (Proof), MPa 130 to 590
110 to 260