C77300 nickel silver belongs to the copper alloys classification, while EN 2.4879 cast nickel belongs to the nickel alloys. There are 20 material properties with values for both materials. Properties with values for just one material (10, in this case) are not shown.

For each property being compared, the top bar is C77300 nickel silver and the bottom bar is EN 2.4879 cast nickel.

Metric UnitsUS Customary Units

Mechanical Properties

Elastic (Young's, Tensile) Modulus, GPa 110
200
Poisson's Ratio 0.3
0.28
Shear Modulus, GPa 42
80
Tensile Strength: Ultimate (UTS), MPa 540
490

Thermal Properties

Latent Heat of Fusion, J/g 180
330
Maximum Temperature: Mechanical, °C 130
1150
Melting Completion (Liquidus), °C 940
1450
Melting Onset (Solidus), °C 920
1400
Specific Heat Capacity, J/kg-K 390
460
Thermal Expansion, µm/m-K 20
13

Otherwise Unclassified Properties

Base Metal Price, % relative 26
55
Density, g/cm3 7.9
8.5
Embodied Carbon, kg CO2/kg material 3.5
8.3
Embodied Energy, MJ/kg 56
120
Embodied Water, L/kg 310
270

Common Calculations

Stiffness to Weight: Axial, points 7.7
13
Stiffness to Weight: Bending, points 20
23
Strength to Weight: Axial, points 19
16
Strength to Weight: Bending, points 19
16
Thermal Shock Resistance, points 17
13

Alloy Composition

Aluminum (Al), % 0 to 0.010
0
Carbon (C), % 0
0.35 to 0.55
Chromium (Cr), % 0
27 to 30
Copper (Cu), % 46 to 50
0
Iron (Fe), % 0
9.4 to 20.7
Lead (Pb), % 0 to 0.050
0
Manganese (Mn), % 0
0 to 1.5
Molybdenum (Mo), % 0
0 to 0.5
Nickel (Ni), % 9.0 to 11
47 to 50
Phosphorus (P), % 0 to 0.25
0 to 0.040
Silicon (Si), % 0.040 to 0.25
1.0 to 2.0
Sulfur (S), % 0
0 to 0.030
Tungsten (W), % 0
4.0 to 6.0
Zinc (Zn), % 37.9 to 45
0
Residuals, % 0 to 0.5
0