C77300 Nickel Silver vs. K93600 Alloy
C77300 nickel silver belongs to the copper alloys classification, while K93600 alloy belongs to the iron alloys. There are 14 material properties with values for both materials. Properties with values for just one material (17, in this case) are not shown.
For each property being compared, the top bar is C77300 nickel silver and the bottom bar is K93600 alloy.
Metric UnitsUS Customary Units
Mechanical Properties
Elastic (Young's, Tensile) Modulus, GPa | 110 | |
140 |
Tensile Strength: Ultimate (UTS), MPa | 540 | |
480 to 810 |
Thermal Properties
Maximum Temperature: Mechanical, °C | 130 | |
440 |
Melting Onset (Solidus), °C | 920 | |
1430 |
Specific Heat Capacity, J/kg-K | 390 | |
520 |
Thermal Expansion, µm/m-K | 20 | |
7.3 |
Electrical Properties
Electrical Conductivity: Equal Volume, % IACS | 5.5 | |
2.2 |
Electrical Conductivity: Equal Weight (Specific), % IACS | 6.3 | |
2.4 |
Otherwise Unclassified Properties
Density, g/cm3 | 7.9 | |
8.1 |
Common Calculations
Stiffness to Weight: Axial, points | 7.7 | |
9.4 |
Stiffness to Weight: Bending, points | 20 | |
21 |
Strength to Weight: Axial, points | 19 | |
16 to 28 |
Strength to Weight: Bending, points | 19 | |
17 to 24 |
Thermal Shock Resistance, points | 17 | |
34 to 57 |