C78200 Nickel Silver vs. 90-silver 10-tin-oxide
C78200 nickel silver belongs to the copper alloys classification, while 90-silver 10-tin-oxide belongs to the otherwise unclassified metals. There are 6 material properties with values for both materials. Properties with values for just one material (25, in this case) are not shown.
For each property being compared, the top bar is C78200 nickel silver and the bottom bar is 90-silver 10-tin-oxide.
Metric UnitsUS Customary Units
Material Properties
Electrical Conductivity: Equal Volume, % IACS | 11 | |
77 to 82 |
Elongation at Break, % | 3.0 to 40 | |
7.0 to 35 |
Resilience: Ultimate (Unit Rupture Work), MJ/m3 | 18 to 120 | |
20 to 68 |
Shear Strength, MPa | 280 to 400 | |
160 to 170 |
Tensile Strength: Ultimate (UTS), MPa | 370 to 630 | |
230 to 300 |
Tensile Strength: Yield (Proof), MPa | 170 to 570 | |
120 to 280 |