Mechanical Properties

Elastic (Young's, Tensile) Modulus, GPa 110
190
Elongation at Break, % 15
17 to 18
Poisson's Ratio 0.3
0.29
Shear Modulus, GPa 43
73
Shear Strength, MPa 290
360 to 410
Tensile Strength: Ultimate (UTS), MPa 480
590 to 670
Tensile Strength: Yield (Proof), MPa 300
350 to 360

Thermal Properties

Latent Heat of Fusion, J/g 180
260
Maximum Temperature: Mechanical, °C 130
410
Melting Completion (Liquidus), °C 930
1450
Melting Onset (Solidus), °C 880
1410
Specific Heat Capacity, J/kg-K 390
470
Thermal Conductivity, W/m-K 36
52
Thermal Expansion, µm/m-K 21
13

Electrical Properties

Electrical Conductivity: Equal Volume, % IACS 7.0
7.3
Electrical Conductivity: Equal Weight (Specific), % IACS 8.0
8.4

Otherwise Unclassified Properties

Base Metal Price, % relative 25
2.1
Density, g/cm3 7.9
7.8
Embodied Carbon, kg CO2/kg material 3.5
1.4
Embodied Energy, MJ/kg 57
19
Embodied Water, L/kg 310
49

Common Calculations

Resilience: Ultimate (Unit Rupture Work), MJ/m3 63
93 to 96
Resilience: Unit (Modulus of Resilience), kJ/m3 400
330 to 350
Stiffness to Weight: Axial, points 7.8
13
Stiffness to Weight: Bending, points 20
24
Strength to Weight: Axial, points 17
21 to 24
Strength to Weight: Bending, points 17
20 to 22
Thermal Diffusivity, mm2/s 12
14
Thermal Shock Resistance, points 15
17 to 20