C95200 bronze belongs to the copper alloys classification, while ASTM A27 cast steel belongs to the iron alloys. There are 28 material properties with values for both materials. Properties with values for just one material (3, in this case) are not shown.

For each property being compared, the top bar is C95200 bronze and the bottom bar is ASTM A27 cast steel.

Metric UnitsUS Customary Units

Mechanical Properties

Elastic (Young's, Tensile) Modulus, GPa 110
190
Elongation at Break, % 29
25 to 27
Poisson's Ratio 0.34
0.29
Shear Modulus, GPa 42
73
Tensile Strength: Ultimate (UTS), MPa 520
460 to 550
Tensile Strength: Yield (Proof), MPa 190
230 to 310

Thermal Properties

Latent Heat of Fusion, J/g 230
250
Maximum Temperature: Mechanical, °C 220
400
Melting Completion (Liquidus), °C 1050
1460
Melting Onset (Solidus), °C 1040
1420
Specific Heat Capacity, J/kg-K 430
470
Thermal Conductivity, W/m-K 50
52
Thermal Expansion, µm/m-K 18
12

Electrical Properties

Electrical Conductivity: Equal Volume, % IACS 11
7.0 to 7.1
Electrical Conductivity: Equal Weight (Specific), % IACS 12
8.1

Otherwise Unclassified Properties

Base Metal Price, % relative 28
1.8
Density, g/cm3 8.3
7.8
Embodied Carbon, kg CO2/kg material 3.0
1.4
Embodied Energy, MJ/kg 50
18
Embodied Water, L/kg 380
45 to 46

Common Calculations

Resilience: Ultimate (Unit Rupture Work), MJ/m3 120
96 to 120
Resilience: Unit (Modulus of Resilience), kJ/m3 170
140 to 260
Stiffness to Weight: Axial, points 7.6
13
Stiffness to Weight: Bending, points 19
24
Strength to Weight: Axial, points 17
16 to 20
Strength to Weight: Bending, points 17
17 to 19
Thermal Diffusivity, mm2/s 14
14
Thermal Shock Resistance, points 19
15 to 18