MakeItFrom.com
Menu (ESC)

C97800 Nickel Silver vs. ASTM A210 Steel

C97800 nickel silver belongs to the copper alloys classification, while ASTM A210 steel belongs to the iron alloys. There are 28 material properties with values for both materials. Properties with values for just one material (3, in this case) are not shown.

For each property being compared, the top bar is C97800 nickel silver and the bottom bar is ASTM A210 steel.

Metric UnitsUS Customary Units

Mechanical Properties

Elastic (Young's, Tensile) Modulus, GPa 130
190
Elongation at Break, % 10
34
Poisson's Ratio 0.33
0.29
Shear Modulus, GPa 48
73
Tensile Strength: Ultimate (UTS), MPa 370
470 to 540
Tensile Strength: Yield (Proof), MPa 170
290 to 310

Thermal Properties

Latent Heat of Fusion, J/g 220
250
Maximum Temperature: Mechanical, °C 230
400
Melting Completion (Liquidus), °C 1180
1460 to 1470
Melting Onset (Solidus), °C 1140
1420
Specific Heat Capacity, J/kg-K 390
470
Thermal Conductivity, W/m-K 25
52 to 53
Thermal Expansion, µm/m-K 16
12

Electrical Properties

Electrical Conductivity: Equal Volume, % IACS 4.0
7.0
Electrical Conductivity: Equal Weight (Specific), % IACS 4.1
8.0 to 8.1

Otherwise Unclassified Properties

Base Metal Price, % relative 40
1.8
Density, g/cm3 8.8
7.9
Embodied Carbon, kg CO2/kg material 5.1
1.4
Embodied Energy, MJ/kg 76
18
Embodied Water, L/kg 330
45 to 46

Common Calculations

Resilience: Ultimate (Unit Rupture Work), MJ/m3 31
140 to 160
Resilience: Unit (Modulus of Resilience), kJ/m3 120
230 to 250
Stiffness to Weight: Axial, points 8.1
13
Stiffness to Weight: Bending, points 19
24
Strength to Weight: Axial, points 12
17 to 19
Strength to Weight: Bending, points 13
17 to 19
Thermal Diffusivity, mm2/s 7.3
14
Thermal Shock Resistance, points 13
15 to 17