K94200 Alloy vs. 88-silver 12-tin-oxide
K94200 alloy belongs to the iron alloys classification, while 88-silver 12-tin-oxide belongs to the otherwise unclassified metals. There are 6 material properties with values for both materials. Properties with values for just one material (17, in this case) are not shown.
For each property being compared, the top bar is K94200 alloy and the bottom bar is 88-silver 12-tin-oxide.
Metric UnitsUS Customary Units
Material Properties
Electrical Conductivity: Equal Volume, % IACS | 2.7 | |
84 to 86 |
Elongation at Break, % | 5.0 to 32 | |
9.0 to 37 |
Resilience: Ultimate (Unit Rupture Work), MJ/m3 | 35 to 130 | |
24 to 70 |
Shear Strength, MPa | 330 to 410 | |
150 to 160 |
Tensile Strength: Ultimate (UTS), MPa | 500 to 710 | |
230 to 280 |
Tensile Strength: Yield (Proof), MPa | 270 to 650 | |
110 to 260 |