K94200 Alloy vs. 92-silver 8-tin-oxide
K94200 alloy belongs to the iron alloys classification, while 92-silver 8-tin-oxide belongs to the otherwise unclassified metals. There are 6 material properties with values for both materials. Properties with values for just one material (17, in this case) are not shown.
For each property being compared, the top bar is K94200 alloy and the bottom bar is 92-silver 8-tin-oxide.
Metric UnitsUS Customary Units
Material Properties
Electrical Conductivity: Equal Volume, % IACS | 2.7 | |
76 to 80 |
Elongation at Break, % | 5.0 to 32 | |
32 to 34 |
Resilience: Ultimate (Unit Rupture Work), MJ/m3 | 35 to 130 | |
62 to 110 |
Shear Strength, MPa | 330 to 410 | |
150 to 210 |
Tensile Strength: Ultimate (UTS), MPa | 500 to 710 | |
230 to 320 |
Tensile Strength: Yield (Proof), MPa | 270 to 650 | |
120 to 300 |