Mechanical Properties
Elastic (Young's, Tensile) Modulus, GPa | 220 | |
100 |
Tensile Strength: Ultimate (UTS), MPa | 1400 | |
340 to 650 |
Thermal Properties
Melting Onset (Solidus), °C | 1320 | |
890 |
Specific Heat Capacity, J/kg-K | 450 | |
380 |
Thermal Conductivity, W/m-K | 11 | |
120 |
Thermal Expansion, µm/m-K | 12 | |
21 |
Otherwise Unclassified Properties
Density, g/cm3 | 8.2 | |
8.1 |
Common Calculations
Stiffness to Weight: Axial, points | 15 | |
7.1 |
Stiffness to Weight: Bending, points | 25 | |
19 |
Strength to Weight: Axial, points | 47 | |
11 to 22 |
Strength to Weight: Bending, points | 34 | |
13 to 21 |
Thermal Diffusivity, mm2/s | 3.0 | |
37 |
Thermal Shock Resistance, points | 38 | |
11 to 22 |