R05200 Tantalum vs. 92-silver 8-tin-oxide
Both R05200 tantalum and 92-silver 8-tin-oxide are otherwise unclassified metals. There are 4 material properties with values for both materials. Properties with values for just one material (18, in this case) are not shown.
For each property being compared, the top bar is R05200 tantalum and the bottom bar is 92-silver 8-tin-oxide.
Metric UnitsUS Customary Units
Material Properties
Elongation at Break, % | 1.1 to 28 | |
32 to 34 |
Resilience: Ultimate (Unit Rupture Work), MJ/m3 | 5.5 to 53 | |
62 to 110 |
Tensile Strength: Ultimate (UTS), MPa | 210 to 540 | |
230 to 320 |
Tensile Strength: Yield (Proof), MPa | 140 to 390 | |
120 to 300 |