R30075 Cobalt vs. ASTM A210 Steel
R30075 cobalt belongs to the cobalt alloys classification, while ASTM A210 steel belongs to the iron alloys. There are 27 material properties with values for both materials. Properties with values for just one material (5, in this case) are not shown.
For each property being compared, the top bar is R30075 cobalt and the bottom bar is ASTM A210 steel.
Metric UnitsUS Customary Units
Mechanical Properties
Elastic (Young's, Tensile) Modulus, GPa | 210 to 250 | |
190 |
Elongation at Break, % | 12 | |
34 |
Fatigue Strength, MPa | 250 to 840 | |
230 to 250 |
Poisson's Ratio | 0.29 | |
0.29 |
Shear Modulus, GPa | 82 to 98 | |
73 |
Tensile Strength: Ultimate (UTS), MPa | 780 to 1280 | |
470 to 540 |
Tensile Strength: Yield (Proof), MPa | 480 to 840 | |
290 to 310 |
Thermal Properties
Latent Heat of Fusion, J/g | 320 | |
250 |
Melting Completion (Liquidus), °C | 1360 | |
1460 to 1470 |
Melting Onset (Solidus), °C | 1290 | |
1420 |
Specific Heat Capacity, J/kg-K | 450 | |
470 |
Thermal Conductivity, W/m-K | 13 | |
52 to 53 |
Thermal Expansion, µm/m-K | 12 | |
12 |
Electrical Properties
Electrical Conductivity: Equal Volume, % IACS | 2.0 | |
7.0 |
Electrical Conductivity: Equal Weight (Specific), % IACS | 2.1 | |
8.0 to 8.1 |
Otherwise Unclassified Properties
Density, g/cm3 | 8.4 | |
7.9 |
Embodied Carbon, kg CO2/kg material | 8.1 | |
1.4 |
Embodied Energy, MJ/kg | 110 | |
18 |
Embodied Water, L/kg | 530 | |
45 to 46 |
Common Calculations
Resilience: Ultimate (Unit Rupture Work), MJ/m3 | 84 to 140 | |
140 to 160 |
Resilience: Unit (Modulus of Resilience), kJ/m3 | 560 to 1410 | |
230 to 250 |
Stiffness to Weight: Axial, points | 14 to 17 | |
13 |
Stiffness to Weight: Bending, points | 24 to 25 | |
24 |
Strength to Weight: Axial, points | 26 to 42 | |
17 to 19 |
Strength to Weight: Bending, points | 22 to 31 | |
17 to 19 |
Thermal Diffusivity, mm2/s | 3.5 | |
14 |
Thermal Shock Resistance, points | 21 to 29 | |
15 to 17 |