R30075 Cobalt vs. ASTM A299 Steel
R30075 cobalt belongs to the cobalt alloys classification, while ASTM A299 steel belongs to the iron alloys. There are 27 material properties with values for both materials. Properties with values for just one material (5, in this case) are not shown.
For each property being compared, the top bar is R30075 cobalt and the bottom bar is ASTM A299 steel.
Metric UnitsUS Customary Units
Mechanical Properties
Elastic (Young's, Tensile) Modulus, GPa | 210 to 250 | |
190 |
Elongation at Break, % | 12 | |
21 to 22 |
Fatigue Strength, MPa | 250 to 840 | |
230 to 250 |
Poisson's Ratio | 0.29 | |
0.29 |
Shear Modulus, GPa | 82 to 98 | |
73 |
Tensile Strength: Ultimate (UTS), MPa | 780 to 1280 | |
590 to 620 |
Tensile Strength: Yield (Proof), MPa | 480 to 840 | |
330 to 360 |
Thermal Properties
Latent Heat of Fusion, J/g | 320 | |
250 |
Melting Completion (Liquidus), °C | 1360 | |
1460 |
Melting Onset (Solidus), °C | 1290 | |
1420 |
Specific Heat Capacity, J/kg-K | 450 | |
470 |
Thermal Conductivity, W/m-K | 13 | |
51 |
Thermal Expansion, µm/m-K | 12 | |
13 |
Electrical Properties
Electrical Conductivity: Equal Volume, % IACS | 2.0 | |
7.2 |
Electrical Conductivity: Equal Weight (Specific), % IACS | 2.1 | |
8.2 |
Otherwise Unclassified Properties
Density, g/cm3 | 8.4 | |
7.8 |
Embodied Carbon, kg CO2/kg material | 8.1 | |
1.4 |
Embodied Energy, MJ/kg | 110 | |
19 |
Embodied Water, L/kg | 530 | |
47 |
Common Calculations
Resilience: Ultimate (Unit Rupture Work), MJ/m3 | 84 to 140 | |
110 |
Resilience: Unit (Modulus of Resilience), kJ/m3 | 560 to 1410 | |
290 to 350 |
Stiffness to Weight: Axial, points | 14 to 17 | |
13 |
Stiffness to Weight: Bending, points | 24 to 25 | |
24 |
Strength to Weight: Axial, points | 26 to 42 | |
21 to 22 |
Strength to Weight: Bending, points | 22 to 31 | |
20 to 21 |
Thermal Diffusivity, mm2/s | 3.5 | |
14 |
Thermal Shock Resistance, points | 21 to 29 | |
17 to 18 |