UHMW-PE vs. ASA
Both UHMW-PE and ASA are thermoplastics. There are 15 material properties with values for both materials. Properties with values for just one material (6, in this case) are not shown.
For each property being compared, the top bar is UHMW-PE and the bottom bar is ASA.
Metric UnitsUS Customary Units
Mechanical Properties
Elastic (Young's, Tensile) Modulus, GPa | 0.8 | |
2.6 |
Elongation at Break, % | 400 | |
6.0 |
Tensile Strength: Ultimate (UTS), MPa | 49 | |
55 |
Thermal Properties
Specific Heat Capacity, J/kg-K | 1750 | |
1300 |
Thermal Conductivity, W/m-K | 0.41 | |
0.18 |
Thermal Expansion, µm/m-K | 180 | |
95 |
Vicat Softening Temperature, °C | 75 | |
96 |
Electrical Properties
Dielectric Constant (Relative Permittivity) At 1 Hz | 2.2 | |
3.7 |
Otherwise Unclassified Properties
Density, g/cm3 | 0.94 | |
1.1 |
Common Calculations
Stiffness to Weight: Axial, points | 0.47 | |
1.3 |
Stiffness to Weight: Bending, points | 33 | |
43 |
Strength to Weight: Axial, points | 14 | |
14 |
Strength to Weight: Bending, points | 32 | |
30 |
Thermal Diffusivity, mm2/s | 0.25 | |
0.13 |
Thermal Shock Resistance, points | 25 | |
16 |