UHMW-PE vs. Ionomer

Both UHMW-PE and ionomer are thermoplastics. There are 11 material properties with values for both materials. Properties with values for just one material (9, in this case) are not shown.

For each property being compared, the top bar is UHMW-PE and the bottom bar is ionomer.

Metric UnitsUS Customary Units

Mechanical Properties

Elastic (Young's, Tensile) Modulus, GPa 0.8
0.4
Elongation at Break, % 400
350
Tensile Strength: Ultimate (UTS), MPa 49
37

Thermal Properties

Melting Onset (Solidus), °C 130
94
Vicat Softening Temperature, °C 75
72

Electrical Properties

Dielectric Constant (Relative Permittivity) At 1 Hz 2.2
2.4

Otherwise Unclassified Properties

Density, g/cm3 0.94
0.94

Common Calculations

Stiffness to Weight: Axial, points 0.47
0.24
Stiffness to Weight: Bending, points 33
26
Strength to Weight: Axial, points 14
11
Strength to Weight: Bending, points 32
26