MakeItFrom.com
Menu (ESC)

UHMW-PE vs. PBI

UHMW-PE belongs to the thermoplastics classification, while PBI belongs to the thermoset plastics. There are 14 material properties with values for both materials. Properties with values for just one material (18, in this case) are not shown.

For each property being compared, the top bar is UHMW-PE and the bottom bar is PBI.

Metric UnitsUS Customary Units

Mechanical Properties

Elastic (Young's, Tensile) Modulus, GPa 0.8
5.9
Elongation at Break, % 400
3.0
Tensile Strength: Ultimate (UTS), MPa 49
160

Thermal Properties

Specific Heat Capacity, J/kg-K 1750
930
Thermal Conductivity, W/m-K 0.41
0.41
Thermal Expansion, µm/m-K 180
23

Electrical Properties

Dielectric Constant (Relative Permittivity) At 1 Hz 2.2
3.4

Otherwise Unclassified Properties

Density, g/cm3 0.94
1.3

Common Calculations

Stiffness to Weight: Axial, points 0.47
2.5
Stiffness to Weight: Bending, points 33
46
Strength to Weight: Axial, points 14
34
Strength to Weight: Bending, points 32
50
Thermal Diffusivity, mm2/s 0.25
0.34
Thermal Shock Resistance, points 25
84