Work Hardened 85-platinum 15-iridium vs. Work Hardened 90-silver 10-tin-oxide
Both work hardened 85-platinum 15-iridium and work hardened 90-silver 10-tin-oxide are otherwise unclassified metals. Both are furnished in the cold worked (strain hardened) condition. There are 4 material properties with values for both materials. Properties with values for just one material (17, in this case) are not shown.
For each property being compared, the top bar is work hardened 85-platinum 15-iridium and the bottom bar is work hardened 90-silver 10-tin-oxide.
Metric UnitsUS Customary Units
Material Properties
Electrical Conductivity: Equal Volume, % IACS | 6.2 | |
77 |
Elongation at Break, % | 5.5 | |
7.0 |
Shear Strength, MPa | 420 | |
170 |
Tensile Strength: Ultimate (UTS), MPa | 730 | |
300 |