30% Glass Fiber (30 GF) PET

30 GF PET is a grade of PET. The graph bars on the material properties cards below compare 30 GF PET to: polyester plastics (top), all thermoplastics (middle), and the entire database (bottom). A full bar means this is the highest value in the relevant set. A half-full bar means it's 50% of the highest, and so on.

Mechanical Properties

Elastic (Young's, Tensile) Modulus

11 GPa 1.6 x 106 psi

Elongation at Break

4.5 %

Flexural Modulus

8.3 GPa 1.2 x 106 psi

Impact Strength: Notched Izod

85 J/m 1.6 ft-lb/in

Tensile Strength: Ultimate (UTS)

140 MPa 20 x 103 psi

Thermal Properties

Glass Transition Temperature

70 °C 160 °F

Maximum Temperature: Autoignition

410 °C 760 °F

Maximum Temperature: Decomposition

390 °C 730 °F

Maximum Temperature: Mechanical

80 °C 180 °F

Melting Onset (Solidus)

260 °C 490 °F

Specific Heat Capacity

1020 J/kg-K 0.24 BTU/lb-°F

Other Material Properties

Density

1.6 g/cm3 97 lb/ft3

Dielectric Constant (Relative Permittivity) At 1 Hz

3.7

Limiting Oxygen Index (LOI)

21 %

Water Absorption At Saturation

0.24 %

Common Calculations

Stiffness to Weight: Axial

3.9 points

Stiffness to Weight: Bending

48 points

Strength to Weight: Axial

25 points

Strength to Weight: Bending

38 points

Followup Questions

Further Reading

Reinforced Plastics Durability, Geoffrey Pritchard (editor), 1999

SPI Plastics Engineering Handbook of the Society of the Plastics Industry, Inc., 5th ed., Michael L. Berins (editor), 2000

Modern Plastics Handbook, Charles A. Harper (editor), 1999

Plastics Materials, 7th ed., J. A. Brydson, 1999