MakeItFrom.com
Menu (ESC)

30% Glass Fiber (30 GF) Thermoplastic Polyimide (PI)

30 GF thermoplastic PI is a grade of thermoplastic PI. The graph bars on the material properties cards below compare 30 GF thermoplastic PI to: imide plastics (top), all thermoplastics (middle), and the entire database (bottom). A full bar means this is the highest value in the relevant set. A half-full bar means it's 50% of the highest, and so on.

Mechanical Properties

Elastic (Young's, Tensile) Modulus

11 GPa 1.6 x 106 psi

Elongation at Break

3.3 %

Flexural Modulus

10 GPa 1.5 x 106 psi

Flexural Strength

270 MPa 39 x 103 psi

Tensile Strength: Ultimate (UTS)

180 MPa 25 x 103 psi

Thermal Properties

Glass Transition Temperature

260 °C 500 °F

Maximum Temperature: Autoignition

600 °C 1110 °F

Maximum Temperature: Decomposition

530 °C 980 °F

Specific Heat Capacity

990 J/kg-K 0.24 BTU/lb-°F

Otherwise Unclassified Properties

Density

1.5 g/cm3 96 lb/ft3

Limiting Oxygen Index (LOI)

35 %

Common Calculations

Stiffness to Weight: Axial

4.0 points

Stiffness to Weight: Bending

48 points

Strength to Weight: Axial

32 points

Strength to Weight: Bending

45 points

Followup Questions

Further Reading

Reinforced Plastics Durability, Geoffrey Pritchard (editor), 1999

SPI Plastics Engineering Handbook of the Society of the Plastics Industry, Inc., 5th ed., Michael L. Berins (editor), 2000

Modern Plastics Handbook, Charles A. Harper (editor), 1999

Plastics Materials, 7th ed., J. A. Brydson, 1999