40% Glass Fiber (40 GF) SAN

40 GF SAN is a grade of SAN. The graph bars on the material properties cards below compare 40 GF SAN to: styrenic plastics (top), all thermoplastics (middle), and the entire database (bottom). A full bar means this is the highest value in the relevant set. A half-full bar means it's 50% of the highest, and so on.

Mechanical Properties

Elongation at Break

2.5 %

Flexural Modulus

13 GPa 1.9 x 106 psi

Impact Strength: Notched Izod

60 J/m 1.1 ft-lb/in

Tensile Strength: Ultimate (UTS)

130 MPa 19 x 103 psi

Other Material Properties

Density

1.4 g/cm3 87 lb/ft3

Specific Heat Capacity

1070 J/kg-K 0.26 BTU/lb-°F

Water Absorption At Saturation

0.28 %

Common Calculations

Strength to Weight: Axial

25 points

Strength to Weight: Bending

40 points

Followup Questions

Further Reading

Reinforced Plastics Durability, Geoffrey Pritchard (editor), 1999

SPI Plastics Engineering Handbook of the Society of the Plastics Industry, Inc., 5th ed., Michael L. Berins (editor), 2000

Modern Plastics Handbook, Charles A. Harper (editor), 1999

Plastics Materials, 7th ed., J. A. Brydson, 1999