6065-T6 aluminum is 6065 aluminum in the T6 temper. To achieve this temper, the metal is solution heat-treated and artificially aged until it meets standard mechanical property requirements. It has the lowest strength and highest ductility compared to the other variants of 6065 aluminum.

The graph bars on the material properties cards below compare 6065-T6 aluminum to: 6000-series alloys (top), all aluminum alloys (middle), and the entire database (bottom). A full bar means this is the highest value in the relevant set. A half-full bar means it's 50% of the highest, and so on.

Mechanical Properties

Elastic (Young's, Tensile) Modulus

68 GPa 9.9 x 106 psi

Elongation at Break

11 %

Fatigue Strength

110 MPa 16 x 103 psi

Poisson's Ratio

0.33

Shear Modulus

26 GPa 3.7 x 106 psi

Shear Strength

190 MPa 27 x 103 psi

Tensile Strength: Ultimate (UTS)

310 MPa 45 x 103 psi

Tensile Strength: Yield (Proof)

270 MPa 39 x 103 psi

Thermal Properties

Latent Heat of Fusion

400 J/g

Maximum Temperature: Mechanical

180 °C 350 °F

Melting Completion (Liquidus)

640 °C 1180 °F

Melting Onset (Solidus)

590 °C 1090 °F

Specific Heat Capacity

890 J/kg-K 0.21 BTU/lb-°F

Thermal Conductivity

170 W/m-K 97 BTU/h-ft-°F

Thermal Expansion

23 µm/m-K

Electrical Properties

Electrical Conductivity: Equal Volume

43 % IACS

Electrical Conductivity: Equal Weight (Specific)

140 % IACS

Otherwise Unclassified Properties

Base Metal Price

11 % relative

Density

2.8 g/cm3 170 lb/ft3

Embodied Carbon

8.4 kg CO2/kg material

Embodied Energy

150 MJ/kg 66 x 103 BTU/lb

Embodied Water

1200 L/kg 140 gal/lb

Common Calculations

Resilience: Ultimate (Unit Rupture Work)

34 MJ/m3

Resilience: Unit (Modulus of Resilience)

540 kJ/m3

Stiffness to Weight: Axial

14 points

Stiffness to Weight: Bending

49 points

Strength to Weight: Axial

31 points

Strength to Weight: Bending

36 points

Thermal Diffusivity

67 mm2/s

Thermal Shock Resistance

14 points

Alloy Composition

Aluminum (Al)Al 94.4 to 98.2
Bismuth (Bi)Bi 0.5 to 1.5
Magnesium (Mg)Mg 0.8 to 1.2
Silicon (Si)Si 0.4 to 0.8
Iron (Fe)Fe 0 to 0.7
Copper (Cu)Cu 0.15 to 0.4
Zinc (Zn)Zn 0 to 0.25
Manganese (Mn)Mn 0 to 0.15
Chromium (Cr)Cr 0 to 0.15
Zirconium (Zr)Zr 0 to 0.15
Titanium (Ti)Ti 0 to 0.1
Lead (Pb)Pb 0 to 0.050
Residualsres. 0 to 0.15

All values are % weight. Ranges represent what is permitted under applicable standards.

Followup Questions

Further Reading

Handbook of Aluminum vol. 2: Alloy Production and Materials Manufacturing, George Totten and D. Scott MacKenzie (editors), 2003

EN 754-2: Aluminium and aluminium alloys. Cold drawn rod/bar and tube. Mechanical properties

Aluminum: Properties and Physical Metallurgy, John E. Hatch (editor), 1984

EN 755-2: Aluminium and aluminium alloys. Extruded rod/bar, tube and profiles. Mechanical properties

EN 573-3: Aluminium and aluminium alloys. Chemical composition and form of wrought products. Chemical composition and form of products