MakeItFrom.com
Menu (ESC)

ASTM A387 Grade 5 Class 1 Steel

ASTM A387 grade 5 class 1 is ASTM A387 grade 5 steel in the annealed condition. The graph bars on the material properties cards below compare ASTM A387 grade 5 class 1 to: wrought alloy steels in the same category (top), all iron alloys (middle), and the entire database (bottom). A full bar means this is the highest value in the relevant set. A half-full bar means it's 50% of the highest, and so on.

Mechanical Properties

Brinell Hardness

150

Elastic (Young's, Tensile) Modulus

190 GPa 28 x 106 psi

Elongation at Break

20 %

Fatigue Strength

160 MPa 23 x 103 psi

Poisson's Ratio

0.29

Shear Modulus

74 GPa 11 x 106 psi

Shear Strength

310 MPa 45 x 103 psi

Tensile Strength: Ultimate (UTS)

500 MPa 73 x 103 psi

Tensile Strength: Yield (Proof)

230 MPa 34 x 103 psi

Thermal Properties

Latent Heat of Fusion

260 J/g

Maximum Temperature: Mechanical

510 °C 950 °F

Melting Completion (Liquidus)

1460 °C 2660 °F

Melting Onset (Solidus)

1420 °C 2590 °F

Specific Heat Capacity

470 J/kg-K 0.11 BTU/lb-°F

Thermal Conductivity

40 W/m-K 23 BTU/h-ft-°F

Thermal Expansion

13 µm/m-K

Electrical Properties

Electrical Conductivity: Equal Volume

8.0 % IACS

Electrical Conductivity: Equal Weight (Specific)

9.2 % IACS

Otherwise Unclassified Properties

Base Metal Price

4.3 % relative

Density

7.8 g/cm3 490 lb/ft3

Embodied Carbon

1.7 kg CO2/kg material

Embodied Energy

23 MJ/kg 10 x 103 BTU/lb

Embodied Water

69 L/kg 8.2 gal/lb

Common Calculations

PREN (Pitting Resistance)

6.8

Resilience: Ultimate (Unit Rupture Work)

83 MJ/m3

Resilience: Unit (Modulus of Resilience)

140 kJ/m3

Stiffness to Weight: Axial

14 points

Stiffness to Weight: Bending

25 points

Strength to Weight: Axial

18 points

Strength to Weight: Bending

18 points

Thermal Diffusivity

11 mm2/s

Thermal Shock Resistance

14 points

Alloy Composition

Iron (Fe)Fe 92.1 to 95.3
Chromium (Cr)Cr 4.0 to 6.0
Molybdenum (Mo)Mo 0.45 to 0.65
Manganese (Mn)Mn 0.3 to 0.6
Silicon (Si)Si 0 to 0.5
Carbon (C)C 0 to 0.15
Phosphorus (P)P 0 to 0.025
Sulfur (S)S 0 to 0.025

All values are % weight. Ranges represent what is permitted under applicable standards.

Followup Questions

Further Reading

ASTM A387: Standard Specification for Pressure Vessel Plates, Alloy Steel, Chromium-Molybdenum

Pressure Vessels: External Pressure Technology, 2nd ed., Carl T. F. Ross, 2011

ASM Specialty Handbook: Carbon and Alloy Steels, J. R. Davis (editor), 1996

Manufacture and Uses of Alloy Steels, Henry D. Hibbard, 2005

Steels: Processing, Structure, and Performance, 2nd ed., George Krauss, 2015