The graph bars on the material properties cards below compare ASTM B817 type I grade 2 class B to: powder metallurgy titanium alloys (top), all titanium alloys (middle), and the entire database (bottom). A full bar means this is the highest value in the relevant set. A half-full bar means it's 50% of the highest, and so on.

Mechanical Properties

Elastic (Young's, Tensile) Modulus

100 GPa 15 x 106 psi

Elongation at Break

13 %

Fatigue Strength

520 MPa 75 x 103 psi

Poisson's Ratio

0.32

Reduction in Area

29 %

Shear Modulus

40 GPa 5.8 x 106 psi

Tensile Strength: Ultimate (UTS)

960 MPa 140 x 103 psi

Tensile Strength: Yield (Proof)

860 MPa 130 x 103 psi

Thermal Properties

Latent Heat of Fusion

410 J/g

Maximum Temperature: Mechanical

340 °C 640 °F

Melting Completion (Liquidus)

1600 °C 2920 °F

Melting Onset (Solidus)

1550 °C 2830 °F

Specific Heat Capacity

560 J/kg-K 0.13 BTU/lb-°F

Thermal Conductivity

7.1 W/m-K 4.1 BTU/h-ft-°F

Thermal Expansion

9.6 µm/m-K

Electrical Properties

Electrical Conductivity: Equal Volume

1.0 % IACS

Electrical Conductivity: Equal Weight (Specific)

2.0 % IACS

Otherwise Unclassified Properties

Base Metal Price

36 % relative

Density

4.4 g/cm3 280 lb/ft3

Embodied Carbon

38 kg CO2/kg material

Embodied Energy

610 MJ/kg 260 x 103 BTU/lb

Embodied Water

200 L/kg 23 gal/lb

Common Calculations

Resilience: Ultimate (Unit Rupture Work)

120 MJ/m3

Resilience: Unit (Modulus of Resilience)

3540 kJ/m3

Stiffness to Weight: Axial

13 points

Stiffness to Weight: Bending

35 points

Strength to Weight: Axial

60 points

Strength to Weight: Bending

49 points

Thermal Diffusivity

2.9 mm2/s

Thermal Shock Resistance

68 points

Alloy Composition

Titanium (Ti)Ti 87 to 91
Aluminum (Al)Al 5.5 to 6.8
Vanadium (V)V 3.5 to 4.5
Iron (Fe)Fe 0 to 0.4
Oxygen (O)O 0 to 0.3
Sodium (Na)Na 0 to 0.2
Chlorine (Cl)Cl 0 to 0.2
Carbon (C)C 0 to 0.1
Silicon (Si)Si 0 to 0.1
Nitrogen (N)N 0 to 0.040
Hydrogen (H)H 0 to 0.015
Residualsres. 0 to 0.4

All values are % weight. Ranges represent what is permitted under applicable standards.

Followup Questions

Further Reading

ASTM B817: Standard Specification for Powder Metallurgy (P/M) Titanium Alloy Structural Components

Titanium and Titanium Alloys: Fundamentals and Applications, Christoph Leyens and Manfred Peters (editors), 2003

Titanium, 2nd ed., G. Lutjering and J. C. Williams, 2007