ASTM D704 type 10 is a grade of melamine moulding compound. The graph bars on the material properties cards below compare ASTM D704 type 10 to other thermoset plastics (top) and the entire database (bottom). A full bar means this is the highest value in the relevant set. A half-full bar means it's 50% of the highest, and so on.

Thermal Properties

Heat Deflection Temperature At 1.82 MPa (264 psi)

190 °C 370 °F

Solidification (Pattern Maker's) Shrinkage

0.26 %

Electrical Properties

Dielectric Strength (Breakdown Potential)

10 kV/mm 0.4 V/mil

Electrical Dissipation At 1 MHz

0.017

Other Material Properties

Density

1.9 g/cm3 120 lb/ft3

Flexural Strength

93 MPa 13 x 103 psi

Water Absorption After 24 Hours

0.17 %

Followup Questions

Further Reading

ASTM D704: Standard Specification for Melamine-Formaldehyde Molding Compounds

Thermosets: Structure, Properties and Applications, Qipeng Guo (editor), 2012

CRC Materials Science and Engineering Handbook, 4th ed., James F. Shackelford et al. (editors), 2015