ASTM D787 Grade 9 Ethyl Cellulose

Grade 9 EC is a grade of Ethyl Cellulose. The graph bars on the material properties cards below compare grade 9 EC to: cellulosic plastics (top), all thermoplastics (middle), and the entire database (bottom). A full bar means this is the highest value in the relevant set. A half-full bar means it's 50% of the highest, and so on.

Mechanical Properties

Impact Strength: Notched Izod

210 J/m 3.9 ft-lb/in

Rockwell R Hardness

84

Tensile Strength: Ultimate (UTS)

24 MPa 3.4 x 103 psi

Thermal Properties

Heat Deflection Temperature At 1.82 MPa (264 psi)

81 °C 180 °F

Heat Deflection Temperature At 455 kPa (66 psi)

92 °C 200 °F

Otherwise Unclassified Properties

Density

1.1 g/cm3 69 lb/ft3

Water Absorption After 24 Hours

1.3 %

Common Calculations

Strength to Weight: Axial

5.9 points

Strength to Weight: Bending

16 points