Annealed 90-Silver 10-Tin-Oxide Alloy

Annealed 90-silver 10-tin-oxide is 90-silver 10-tin-oxide in the annealed condition. The graph bars on the material properties cards below compare annealed 90-silver 10-tin-oxide to: precious metal electrical contact alloys (top), all alloys in the same category (middle), and the entire database (bottom). A full bar means this is the highest value in the relevant set. A half-full bar means it's 50% of the highest, and so on.

Mechanical Properties

Elongation at Break

35 %

Shear Strength

160 MPa 23 x 103 psi

Tensile Strength: Ultimate (UTS)

230 MPa 34 x 103 psi

Tensile Strength: Yield (Proof)

120 MPa 17 x 103 psi

Other Material Properties

Electrical Conductivity: Equal Volume

82 % IACS

Common Calculations

Resilience: Ultimate (Unit Rupture Work)

68 MJ/m3