Conditioned PA 11 is a grade of PA 11. The graph bars on the material properties cards below compare conditioned PA 11 to: polyamide plastics (top), all thermoplastics (middle), and the entire database (bottom). A full bar means this is the highest value in the relevant set. A half-full bar means it's 50% of the highest, and so on.

Mechanical Properties

Elastic (Young's, Tensile) Modulus

0.4 GPa 0.058 x 106 psi

Elongation at Break

80 %

Tensile Strength: Ultimate (UTS)

25 MPa 3.6 x 103 psi

Thermal Properties

Melting Onset (Solidus)

180 °C 360 °F

Specific Heat Capacity

1740 J/kg-K 0.42 BTU/lb-°F

Thermal Conductivity

0.28 W/m-K 0.16 BTU/h-ft-°F

Otherwise Unclassified Properties

Density

1.0 g/cm3 64 lb/ft3

Limiting Oxygen Index (LOI)

29 %

Common Calculations

Stiffness to Weight: Axial

0.22 points

Stiffness to Weight: Bending

24 points

Strength to Weight: Axial

6.7 points

Strength to Weight: Bending

18 points

Thermal Diffusivity

0.16 mm2/s

Followup Questions

Further Reading

SPI Plastics Engineering Handbook of the Society of the Plastics Industry, Inc., 5th ed., Michael L. Berins (editor), 2000

Modern Plastics Handbook, Charles A. Harper (editor), 1999

Plastics Materials, 7th ed., J. A. Brydson, 1999