EA rubber is a thermoset elastomer or rubber material. The graph bars on the material properties cards below compare EA rubber to other rubber materials (top) and the entire database (bottom). A full bar means this is the highest value in the relevant set. A half-full bar means it's 50% of the highest, and so on.
Mechanical Properties
Elongation at Break
430 %
Tensile Strength: Ultimate (UTS)
14 MPa 2.0 x 103 psi
Other Material Properties
Density
1.3 g/cm3 79 lb/ft3
Maximum Temperature: Mechanical
160 °C 320 °F
Common Calculations
Strength to Weight: Axial
3.0 points
Strength to Weight: Bending
10 points