The graph bars on the material properties cards below compare full-hard 90-silver 10-cadmium-oxide to: precious metal electrical contact alloys (top), all alloys in the same category (middle), and the entire database (bottom). A full bar means this is the highest value in the relevant set. A half-full bar means it's 50% of the highest, and so on.

Mechanical Properties

Elongation at Break

1.1 %

Shear Strength

230 MPa 33 x 103 psi

Tensile Strength: Ultimate (UTS)

400 MPa 58 x 103 psi

Other Material Properties

Density

10 g/cm3 640 lb/ft3

Electrical Conductivity: Equal Volume

72 % IACS

Electrical Conductivity: Equal Weight (Specific)

64 % IACS

Common Calculations

Strength to Weight: Axial

11 points

Strength to Weight: Bending

12 points