H80 C12200 copper is C12200 copper in the H80 (hard drawn) temper. The graph bars on the material properties cards below compare H80 C12200 copper to: wrought coppers (top), all copper alloys (middle), and the entire database (bottom). A full bar means this is the highest value in the relevant set. A half-full bar means it's 50% of the highest, and so on.

Mechanical Properties

Elastic (Young's, Tensile) Modulus

120 GPa 17 x 106 psi

Elongation at Break

7.8 %

Poisson's Ratio

0.34

Shear Modulus

43 GPa 6.3 x 106 psi

Shear Strength

210 MPa 30 x 103 psi

Tensile Strength: Ultimate (UTS)

350 MPa 51 x 103 psi

Tensile Strength: Yield (Proof)

310 MPa 45 x 103 psi

Thermal Properties

Latent Heat of Fusion

210 J/g

Maximum Temperature: Mechanical

200 °C 390 °F

Melting Completion (Liquidus)

1080 °C 1980 °F

Melting Onset (Solidus)

1030 °C 1880 °F

Specific Heat Capacity

390 J/kg-K 0.092 BTU/lb-°F

Thermal Conductivity

340 W/m-K 200 BTU/h-ft-°F

Thermal Expansion

17 µm/m-K

Electrical Properties

Electrical Conductivity: Equal Volume

85 % IACS

Electrical Conductivity: Equal Weight (Specific)

85 % IACS

Otherwise Unclassified Properties

Base Metal Price

31 % relative

Density

9.0 g/cm3 560 lb/ft3

Embodied Carbon

2.6 kg CO2/kg material

Embodied Energy

41 MJ/kg 18 x 103 BTU/lb

Embodied Water

310 L/kg 37 gal/lb

Common Calculations

Resilience: Ultimate (Unit Rupture Work)

27 MJ/m3

Resilience: Unit (Modulus of Resilience)

410 kJ/m3

Stiffness to Weight: Axial

7.2 points

Stiffness to Weight: Bending

18 points

Strength to Weight: Axial

11 points

Strength to Weight: Bending

12 points

Thermal Diffusivity

98 mm2/s

Thermal Shock Resistance

13 points

Alloy Composition

Copper (Cu)Cu 99.9 to 99.985
Phosphorus (P)P 0.015 to 0.040

All values are % weight. Ranges represent what is permitted under applicable standards.

Followup Questions

Further Reading

ASTM B111: Standard Specification for Copper and Copper-Alloy Seamless Condenser Tubes and Ferrule Stock

Copper Alloys: Preparation, Properties and Applications, Michael Naboka and Jennifer Giordano (editors), 2013

Copper: Its Trade, Manufacture, Use, and Environmental Status, Gunter Joseph, 2001

Properties and Selection: Nonferrous Alloys and Special-Purpose Materials, ASM Handbook vol. 2, ASM International, 1993