Hardened SAE-AISI S2 is SAE-AISI S2 steel in the hardened (H) condition. The graph bars on the material properties cards below compare hardened SAE-AISI S2 to: tool steels (top), all iron alloys (middle), and the entire database (bottom). A full bar means this is the highest value in the relevant set. A half-full bar means it's 50% of the highest, and so on.

Mechanical Properties

Elastic (Young's, Tensile) Modulus

190 GPa 27 x 106 psi

Poisson's Ratio

0.29

Rockwell C Hardness

60

Shear Modulus

72 GPa 10 x 106 psi

Tensile Strength: Ultimate (UTS)

1940 MPa 280 x 103 psi

Thermal Properties

Latent Heat of Fusion

260 J/g

Melting Completion (Liquidus)

1450 °C 2640 °F

Melting Onset (Solidus)

1410 °C 2570 °F

Specific Heat Capacity

470 J/kg-K 0.11 BTU/lb-°F

Thermal Conductivity

44 W/m-K 25 BTU/h-ft-°F

Thermal Expansion

11 µm/m-K

Electrical Properties

Electrical Conductivity: Equal Volume

7.4 % IACS

Electrical Conductivity: Equal Weight (Specific)

8.5 % IACS

Otherwise Unclassified Properties

Base Metal Price

2.6 % relative

Density

7.8 g/cm3 490 lb/ft3

Embodied Carbon

2.1 kg CO2/kg material

Embodied Energy

30 MJ/kg 13 x 103 BTU/lb

Embodied Water

49 L/kg 5.8 gal/lb

Common Calculations

Stiffness to Weight: Axial

13 points

Stiffness to Weight: Bending

24 points

Strength to Weight: Axial

69 points

Strength to Weight: Bending

44 points

Thermal Diffusivity

12 mm2/s

Thermal Shock Resistance

68 points

Alloy Composition

Iron (Fe)Fe 96 to 98.1
Silicon (Si)Si 0.9 to 1.2
Carbon (C)C 0.4 to 0.55
Molybdenum (Mo)Mo 0.3 to 0.6
Manganese (Mn)Mn 0.3 to 0.5
Vanadium (V)V 0 to 0.5
Nickel (Ni)Ni 0 to 0.3
Copper (Cu)Cu 0 to 0.25
Phosphorus (P)P 0 to 0.030
Sulfur (S)S 0 to 0.030

All values are % weight. Ranges represent what is permitted under applicable standards.

Followup Questions

Further Reading

SAE J437: Selection and Heat Treatment of Tool and Die Steels

ASTM A681: Standard Specification for Tool Steels Alloy

Tool Steels, 5th ed., George Roberts et al., 1998

Tool Steels: Properties and Performance, Rafael A. Mesquita (editor), 2016

ASM Specialty Handbook: Carbon and Alloy Steels, J. R. Davis (editor), 1996