NEMA grade G-5 is a grade of NEMA laminate. The graph bars on the material properties cards below compare NEMA grade G-5 to other thermoset plastics (top) and the entire database (bottom). A full bar means this is the highest value in the relevant set. A half-full bar means it's 50% of the highest, and so on.

Mechanical Properties

Compressive (Crushing) Strength

330 MPa 47 x 103 psi

Flexural Modulus

16 GPa 2.3 x 106 psi

Flexural Strength

310 MPa 45 x 103 psi

Impact Strength: Notched Izod

330 J/m 6.3 ft-lb/in

Rockwell M Hardness

120

Shear Strength

140 MPa 20 x 103 psi

Tensile Strength: Ultimate (UTS)

230 MPa 34 x 103 psi

Thermal Properties

Maximum Temperature: Mechanical

140 °C 280 °F

Thermal Expansion

10 µm/m-K

Electrical Properties

Dielectric Constant (Relative Permittivity) At 1 MHz

6.7

Dielectric Strength (Breakdown Potential)

14 kV/mm 0.54 V/mil

Otherwise Unclassified Properties

Density

1.9 g/cm3 120 lb/ft3

Water Absorption After 24 Hours

0.63 %

Common Calculations

Strength to Weight: Axial

34 points

Strength to Weight: Bending

44 points