MakeItFrom.com
Menu (ESC)

Normalized (+N) 1.1127 Steel

EN 1.1127 +N steel is EN 1.1127 steel in the normalized condition. The graph bars on the material properties cards below compare EN 1.1127 +N steel to: wrought carbon or non-alloy steels (top), all iron alloys (middle), and the entire database (bottom). A full bar means this is the highest value in the relevant set. A half-full bar means it's 50% of the highest, and so on.

Mechanical Properties

Brinell Hardness

200

Elastic (Young's, Tensile) Modulus

190 GPa 27 x 106 psi

Elongation at Break

15 %

Fatigue Strength

280 MPa 40 x 103 psi

Poisson's Ratio

0.29

Shear Modulus

73 GPa 11 x 106 psi

Shear Strength

430 MPa 62 x 103 psi

Tensile Strength: Ultimate (UTS)

700 MPa 100 x 103 psi

Tensile Strength: Yield (Proof)

430 MPa 62 x 103 psi

Thermal Properties

Latent Heat of Fusion

250 J/g

Maximum Temperature: Mechanical

400 °C 750 °F

Melting Completion (Liquidus)

1460 °C 2650 °F

Melting Onset (Solidus)

1410 °C 2580 °F

Specific Heat Capacity

470 J/kg-K 0.11 BTU/lb-°F

Thermal Conductivity

49 W/m-K 28 BTU/h-ft-°F

Thermal Expansion

12 µm/m-K

Electrical Properties

Electrical Conductivity: Equal Volume

7.3 % IACS

Electrical Conductivity: Equal Weight (Specific)

8.4 % IACS

Otherwise Unclassified Properties

Base Metal Price

2.1 % relative

Density

7.8 g/cm3 490 lb/ft3

Embodied Carbon

1.5 kg CO2/kg material

Embodied Energy

19 MJ/kg 8.3 x 103 BTU/lb

Embodied Water

49 L/kg 5.8 gal/lb

Common Calculations

Resilience: Ultimate (Unit Rupture Work)

90 MJ/m3

Resilience: Unit (Modulus of Resilience)

490 kJ/m3

Stiffness to Weight: Axial

13 points

Stiffness to Weight: Bending

24 points

Strength to Weight: Axial

25 points

Strength to Weight: Bending

22 points

Thermal Diffusivity

13 mm2/s

Thermal Shock Resistance

22 points

Alloy Composition

Iron (Fe)Fe 96.6 to 98.1
Manganese (Mn)Mn 1.4 to 1.7
Carbon (C)C 0.34 to 0.42
Silicon (Si)Si 0.15 to 0.35
Chromium (Cr)Cr 0 to 0.4
Nickel (Ni)Ni 0 to 0.4
Molybdenum (Mo)Mo 0 to 0.1
Phosphorus (P)P 0 to 0.035
Sulfur (S)S 0 to 0.035

All values are % weight. Ranges represent what is permitted under applicable standards.

Followup Questions

Further Reading

EN 10297-1: Seamless circular steel tubes for mechanical and general engineering purposes - Technical delivery conditions - Part 1: Non-alloy and alloy steel tubes

Carbon Steel Handbook, D. Gandy, 2007

ASM Specialty Handbook: Carbon and Alloy Steels, J. R. Davis (editor), 1996

Ferrous Materials: Steel and Cast Iron, Hans Berns and Werner Theisen, 2008

Steels: Processing, Structure, and Performance, 2nd ed., George Krauss, 2015