Quenched and Tempered (+QT) 1.0619 Steel

EN 1.0619 +QT steel is EN 1.0619 steel in the quenched and tempered condition. The graph bars on the material properties cards below compare EN 1.0619 +QT steel to: cast carbon steels (top), all iron alloys (middle), and the entire database (bottom). A full bar means this is the highest value in the relevant set. A half-full bar means it's 50% of the highest, and so on.

Mechanical Properties

Elastic (Young's, Tensile) Modulus

190 GPa 27 x 106 psi

Elongation at Break

25 %

Fatigue Strength

200 MPa 29 x 103 psi

Impact Strength: V-Notched Charpy

45 J 33 ft-lb

Poisson's Ratio

0.29

Shear Modulus

73 GPa 11 x 106 psi

Tensile Strength: Ultimate (UTS)

510 MPa 74 x 103 psi

Tensile Strength: Yield (Proof)

270 MPa 40 x 103 psi

Thermal Properties

Latent Heat of Fusion

250 J/g

Maximum Temperature: Mechanical

400 °C 750 °F

Melting Completion (Liquidus)

1460 °C 2660 °F

Melting Onset (Solidus)

1420 °C 2580 °F

Specific Heat Capacity

470 J/kg-K 0.11 BTU/lb-°F

Thermal Conductivity

48 W/m-K 28 BTU/h-ft-°F

Thermal Expansion

12 µm/m-K

Electrical Properties

Electrical Conductivity: Equal Volume

7.3 % IACS

Electrical Conductivity: Equal Weight (Specific)

8.4 % IACS

Otherwise Unclassified Properties

Base Metal Price

2.1 % relative

Density

7.8 g/cm3 490 lb/ft3

Embodied Carbon

1.5 kg CO2/kg material

Embodied Energy

20 MJ/kg 8.5 x 103 BTU/lb

Embodied Water

48 L/kg 5.7 gal/lb

Common Calculations

Resilience: Ultimate (Unit Rupture Work)

110 MJ/m3

Resilience: Unit (Modulus of Resilience)

200 kJ/m3

Stiffness to Weight: Axial

13 points

Stiffness to Weight: Bending

24 points

Strength to Weight: Axial

18 points

Strength to Weight: Bending

18 points

Thermal Diffusivity

13 mm2/s

Thermal Shock Resistance

16 points

Alloy Composition

Iron (Fe)Fe 96.6 to 99.32
Manganese (Mn)Mn 0.5 to 1.4
Silicon (Si)Si 0 to 0.6
Carbon (C)C 0.18 to 0.23
Nickel (Ni)Ni 0 to 0.4
Chromium (Cr)Cr 0 to 0.3
Copper (Cu)Cu 0 to 0.3
Molybdenum (Mo)Mo 0 to 0.12
Phosphorus (P)P 0 to 0.030
Vanadium (V)V 0 to 0.030
Sulfur (S)S 0 to 0.020

All values are % weight. Ranges represent what is permitted under applicable standards.

Followup Questions

Further Reading

ISO 4991: Steel castings for pressure purposes

Carbon Steel Handbook, D. Gandy, 2007

Ferrous Materials: Steel and Cast Iron, Hans Berns and Werner Theisen, 2008

Steels: Processing, Structure, and Performance, 2nd ed., George Krauss, 2015