MakeItFrom.com
Menu (ESC)

TD01 Tempered C17200 Copper

TD01 C17200 copper is C17200 copper in the TD01 (solution heat treated and cold worked to quarter-hard) temper. It has the second lowest strength compared to the other variants of C17200 copper. The graph bars on the material properties cards below compare TD01 C17200 copper to: wrought coppers (top), all copper alloys (middle), and the entire database (bottom). A full bar means this is the highest value in the relevant set. A half-full bar means it's 50% of the highest, and so on.

Mechanical Properties

Elastic (Young's, Tensile) Modulus

120 GPa 17 x 106 psi

Elongation at Break

17 %

Poisson's Ratio

0.33

Rockwell B Hardness

79

Rockwell Superficial 30T Hardness

69

Shear Modulus

45 GPa 6.5 x 106 psi

Shear Strength

350 MPa 51 x 103 psi

Tensile Strength: Ultimate (UTS)

570 MPa 82 x 103 psi

Thermal Properties

Latent Heat of Fusion

230 J/g

Maximum Temperature: Mechanical

280 °C 530 °F

Melting Completion (Liquidus)

980 °C 1800 °F

Melting Onset (Solidus)

870 °C 1590 °F

Specific Heat Capacity

390 J/kg-K 0.092 BTU/lb-°F

Thermal Conductivity

110 W/m-K 61 BTU/h-ft-°F

Thermal Expansion

18 µm/m-K

Electrical Properties

Electrical Conductivity: Equal Volume

22 % IACS

Electrical Conductivity: Equal Weight (Specific)

23 % IACS

Otherwise Unclassified Properties

Density

8.8 g/cm3 550 lb/ft3

Embodied Carbon

9.4 kg CO2/kg material

Embodied Energy

150 MJ/kg 63 x 103 BTU/lb

Embodied Water

310 L/kg 37 gal/lb

Common Calculations

Resilience: Ultimate (Unit Rupture Work)

4.2 to 500 MJ/m3

Stiffness to Weight: Axial

7.6 points

Stiffness to Weight: Bending

19 points

Strength to Weight: Axial

18 points

Strength to Weight: Bending

17 points

Thermal Diffusivity

31 mm2/s

Thermal Shock Resistance

19 points

Alloy Composition

Copper (Cu)Cu 96.1 to 98
Beryllium (Be)Be 1.8 to 2.0
Nickel (Ni)Ni 0.2 to 0.6
Iron (Fe)Fe 0 to 0.4
Silicon (Si)Si 0 to 0.2
Aluminum (Al)Al 0 to 0.2
Residualsres. 0 to 0.5

All values are % weight. Ranges represent what is permitted under applicable standards.

Followup Questions

Further Reading

ASTM B194: Standard Specification for Copper-Beryllium Alloy Plate, Sheet, Strip, and Rolled Bar

Copper: Its Trade, Manufacture, Use, and Environmental Status, Gunter Joseph, 2001

Properties and Selection: Nonferrous Alloys and Special-Purpose Materials, ASM Handbook vol. 2, ASM International, 1993