TM00 Mill Hardened C17200 Copper

TM00 C17200 copper is C17200 copper in the TM00 (mill annealed) temper. It has the second highest ductility compared to the other variants of C17200 copper. The graph bars on the material properties cards below compare TM00 C17200 copper to: wrought coppers (top), all copper alloys (middle), and the entire database (bottom). A full bar means this is the highest value in the relevant set. A half-full bar means it's 50% of the highest, and so on.

Mechanical Properties

Elastic (Young's, Tensile) Modulus

120 GPa 17 x 106 psi

Elongation at Break

18 %

Poisson's Ratio

0.33

Rockwell B Hardness

110

Shear Modulus

45 GPa 6.5 x 106 psi

Shear Strength

450 MPa 65 x 103 psi

Tensile Strength: Ultimate (UTS)

730 MPa 110 x 103 psi

Tensile Strength: Yield (Proof)

570 MPa 83 x 103 psi

Thermal Properties

Latent Heat of Fusion

230 J/g

Maximum Temperature: Mechanical

280 °C 530 °F

Melting Completion (Liquidus)

980 °C 1800 °F

Melting Onset (Solidus)

870 °C 1590 °F

Specific Heat Capacity

390 J/kg-K 0.092 BTU/lb-°F

Thermal Conductivity

110 W/m-K 61 BTU/h-ft-°F

Thermal Expansion

18 µm/m-K

Electrical Properties

Electrical Conductivity: Equal Volume

22 % IACS

Electrical Conductivity: Equal Weight (Specific)

23 % IACS

Otherwise Unclassified Properties

Density

8.8 g/cm3 550 lb/ft3

Embodied Carbon

9.4 kg CO2/kg material

Embodied Energy

150 MJ/kg 63 x 103 BTU/lb

Embodied Water

310 L/kg 37 gal/lb

Common Calculations

Resilience: Ultimate (Unit Rupture Work)

120 MJ/m3

Resilience: Unit (Modulus of Resilience)

1350 kJ/m3

Stiffness to Weight: Axial

7.6 points

Stiffness to Weight: Bending

19 points

Strength to Weight: Axial

23 points

Strength to Weight: Bending

20 points

Thermal Diffusivity

31 mm2/s

Thermal Shock Resistance

24 points

Alloy Composition

Copper (Cu)Cu 96.1 to 98
Beryllium (Be)Be 1.8 to 2.0
Nickel (Ni)Ni 0.2 to 0.6
Iron (Fe)Fe 0 to 0.4
Silicon (Si)Si 0 to 0.2
Aluminum (Al)Al 0 to 0.2
Residualsres. 0 to 0.5

All values are % weight. Ranges represent what is permitted under applicable standards.

Followup Questions

Further Reading

ASTM B194: Standard Specification for Copper-Beryllium Alloy Plate, Sheet, Strip, and Rolled Bar

Copper: Its Trade, Manufacture, Use, and Environmental Status, Gunter Joseph, 2001

Properties and Selection: Nonferrous Alloys and Special-Purpose Materials, ASM Handbook vol. 2, ASM International, 1993