MakeItFrom.com
Menu (ESC)

TM04 Mill Hardened C19010 Copper

TM04 C19010 copper is C19010 copper in the TM04 (mill hardened to full-hard) temper. The graph bars on the material properties cards below compare TM04 C19010 copper to: wrought coppers (top), all copper alloys (middle), and the entire database (bottom). A full bar means this is the highest value in the relevant set. A half-full bar means it's 50% of the highest, and so on.

Mechanical Properties

Elastic (Young's, Tensile) Modulus

120 GPa 17 x 106 psi

Elongation at Break

9.2 %

Poisson's Ratio

0.34

Shear Modulus

43 GPa 6.3 x 106 psi

Shear Strength

270 MPa 40 x 103 psi

Tensile Strength: Ultimate (UTS)

460 MPa 67 x 103 psi

Tensile Strength: Yield (Proof)

400 MPa 58 x 103 psi

Thermal Properties

Latent Heat of Fusion

210 J/g

Maximum Temperature: Mechanical

200 °C 400 °F

Melting Completion (Liquidus)

1060 °C 1940 °F

Melting Onset (Solidus)

1010 °C 1850 °F

Specific Heat Capacity

390 J/kg-K 0.093 BTU/lb-°F

Thermal Conductivity

260 W/m-K 150 BTU/h-ft-°F

Thermal Expansion

17 µm/m-K

Electrical Properties

Electrical Conductivity: Equal Volume

50 % IACS

Electrical Conductivity: Equal Weight (Specific)

50 % IACS

Otherwise Unclassified Properties

Base Metal Price

31 % relative

Density

8.9 g/cm3 560 lb/ft3

Embodied Carbon

2.7 kg CO2/kg material

Embodied Energy

42 MJ/kg 18 x 103 BTU/lb

Embodied Water

310 L/kg 37 gal/lb

Common Calculations

Resilience: Ultimate (Unit Rupture Work)

41 MJ/m3

Resilience: Unit (Modulus of Resilience)

680 kJ/m3

Stiffness to Weight: Axial

7.3 points

Stiffness to Weight: Bending

18 points

Strength to Weight: Axial

14 points

Strength to Weight: Bending

15 points

Thermal Diffusivity

75 mm2/s

Thermal Shock Resistance

16 points

Alloy Composition

Copper (Cu)Cu 97.3 to 99.04
Nickel (Ni)Ni 0.8 to 1.8
Silicon (Si)Si 0.15 to 0.35
Phosphorus (P)P 0.010 to 0.050
Residualsres. 0 to 0.5

All values are % weight. Ranges represent what is permitted under applicable standards.

Followup Questions

Further Reading

ASTM B422: Standard Specification for Copper-Aluminum-Silicon-Cobalt Alloy, Copper-Nickel-Silicon-Magnesium Alloy, Copper-Nickel-Silicon Alloy, Copper-Nickel-Aluminum-Magnesium Alloy, and Copper- Nickel-Tin Alloy Sheet and Strip

Copper: Its Trade, Manufacture, Use, and Environmental Status, Gunter Joseph, 2001

ASM Specialty Handbook: Copper and Copper Alloys, J. R. Davis (editor), 2001