2011A Aluminum vs. 92-silver 8-tin-oxide
2011A aluminum belongs to the aluminum alloys classification, while 92-silver 8-tin-oxide belongs to the otherwise unclassified metals. There are 6 material properties with values for both materials. Properties with values for just one material (24, in this case) are not shown.
For each property being compared, the top bar is 2011A aluminum and the bottom bar is 92-silver 8-tin-oxide.
Metric UnitsUS Customary Units
Material Properties
Electrical Conductivity: Equal Volume, % IACS | 33 | |
76 to 80 |
Elongation at Break, % | 6.8 to 16 | |
32 to 34 |
Resilience: Ultimate (Unit Rupture Work), MJ/m3 | 20 to 40 | |
62 to 110 |
Shear Strength, MPa | 190 to 250 | |
150 to 210 |
Tensile Strength: Ultimate (UTS), MPa | 310 to 410 | |
230 to 320 |
Tensile Strength: Yield (Proof), MPa | 140 to 310 | |
120 to 300 |