88-silver 12-tin-oxide vs. ASTM A182 Grade F23

88-silver 12-tin-oxide belongs to the otherwise unclassified metals classification, while ASTM A182 grade F23 belongs to the iron alloys. There are 6 material properties with values for both materials. Properties with values for just one material (27, in this case) are not shown.

For each property being compared, the top bar is 88-silver 12-tin-oxide and the bottom bar is ASTM A182 grade F23.

Metric UnitsUS Customary Units

Material Properties

Electrical Conductivity: Equal Volume, % IACS 84 to 86
7.8
Elongation at Break, % 9.0 to 37
22
Resilience: Ultimate (Unit Rupture Work), MJ/m3 24 to 70
120
Shear Strength, MPa 150 to 160
360
Tensile Strength: Ultimate (UTS), MPa 230 to 280
570
Tensile Strength: Yield (Proof), MPa 110 to 260
460