Material Properties
Density, g/cm3 | 1.1 | |
1.1 to 1.4 |
Dielectric Constant (Relative Permittivity) At 1 Hz | 3.7 | |
2.7 to 3.2 |
Electrical Resistivity Order of Magnitude, 10x Ω-m | 13 | |
15 |
Elongation at Break, % | 6.0 | |
3.5 to 28 |
Specific Heat Capacity, J/kg-K | 1300 | |
1020 to 1250 |
Strength to Weight: Axial, points | 14 | |
16 to 27 |
Strength to Weight: Bending, points | 30 | |
33 to 42 |
Tensile Strength: Ultimate (UTS), MPa | 55 | |
63 to 140 |
Thermal Expansion, µm/m-K | 95 | |
25 to 60 |